Below are some SEM images of the silicon nanostructures achieved by the CORE process:
Below are some SEM images of the silicon nanostructures achieved by the CORE process:


<gallery caption="" perrow="1">
 
[[File:Fig 13a.png|800px]]
[[File:Fig 13a.png|800px]]
[[|thumb|left]] '''''Submicron silicon trenches and lines derived from the fine-tuned CORE sequence.'''''  
[[|thumb|left]] '''''Submicron silicon trenches and lines derived from the fine-tuned CORE sequence.'''''  
Line 31: Line 31:


'''''Notch-free nanostructures in SOI material derived from the fine-tuned CORE sequence Left) Grating with 80 nm periodicity. Right) RIE lag test structure between 30 and 100 nm.'''''