It is not only usable for Al deposition. The thermal evaporator has room for two evaporation sources and thereby the possibility to make thin films of two different metals. At the moment not that many metals have been tested, so right now only Al and Ag can be evaporated. We have attempted to evaporate Au and Zn but these are not standard processes. If you would like to deposit these or other metals, please talk to the Thin Film group. | It is not only usable for Al deposition. The thermal evaporator has room for two evaporation sources and thereby the possibility to make thin films of two different metals. At the moment not that many metals have been tested, so right now only Al and Ag can be evaporated. We have attempted to evaporate Au and Zn but these are not standard processes. If you would like to deposit these or other metals, please talk to the Thin Film group. | ||
Compared to the [[Specific Process Knowledge/Thin film deposition/Wordentec|Wordentec]], the thermal evaporator is quicker to use if you only need to deposit on one wafer or on small samples, as it only takes about 15 minutes to pump down the chamber. You can also deposit thicker layers because the throw distance from source to sample is shorter, so the material use is more efficient: In the thermal evaporator, you get up to | Compared to the [[Specific Process Knowledge/Thin film deposition/Wordentec|Wordentec]], the thermal evaporator is quicker to use if you only need to deposit on one wafer or on small samples, as it only takes about 15 minutes to pump down the chamber. You can also deposit thicker layers because the throw distance from source to sample is shorter, so the material use is more efficient: In the thermal evaporator, you get up to 200 nm per metal pellet, whereas in the Wordentec you get about 15 nm per pellet. However, the thickness uniformity is better for large samples in the Wordentec also because of the longer distance from source to sample. | ||
So if you want a quick deposition process and/or a relatively thick metal layer, and your samples are small or the thickness uniformity is not critical, then the Thermal Evaporator is a very good choice for you. If you need to deposit on many wafers or you need a more constant layer uniformity across a full 4" or 6" wafer, then the Wordentec is best. | So if you want a quick deposition process and/or a relatively thick metal layer, and your samples are small or the thickness uniformity is not critical, then the Thermal Evaporator is a very good choice for you. If you need to deposit on many wafers or you need a more constant layer uniformity across a full 4" or 6" wafer, then the Wordentec is best. | ||