Specific Process Knowledge/Thin film deposition/Deposition of Nickel: Difference between revisions
Appearance
m →Nickel deposition: added link w info on deposition rate |
m →Nickel deposition: about allowed materials in lesker |
||
| Line 121: | Line 121: | ||
* Metals | * Metals | ||
| | | | ||
* | * Almost any that do not outgas. | ||
| | | | ||
*Almost any that do not outgas. Check the cross-contamination sheets in Labmanager. | *Almost any that do not outgas. Check the cross-contamination sheets in Labmanager. | ||
Revision as of 17:12, 21 April 2020
Feedback to this page: click here
Nickel deposition
Nickel can be deposited by e-beam evaporation, sputtering or electroplating. In the chart below you can compare the different deposition equipment.
| E-beam evaporation (Temescal) | E-beam evaporation (Wordentec) | E-beam evaporation (Physimeca) | Sputter deposition (Lesker) | Sputter deposition (Cluster-based sputter system) | Electroplating (Electroplating-Ni) | |
|---|---|---|---|---|---|---|
| General description | E-beam deposition of Nickel | E-beam deposition of Nickel | E-beam deposition of Nickel | Sputter deposition of Nickel | Sputter deposition of Nickel | Electroplating of Nickel |
| Pre-clean | Ar ion bombardment | RF Ar clean | RF Ar clean | RF Ar clean | None | |
| Layer thickness | 10 Å to 1 µm * | 10 Å to 1 µm * | 10 Å to 2000 Å | 10 Å to 5000 Å ** | 10 Å to 5000 Å ** | ~ 20 µm to ~ 1000 µm |
| Deposition rate | 2-10 Å/s | 10-15 Å/s | 1-10 Å/s | Depends on process parameters, about 1 Å/s | Depends on process parameters, at least ~ 4 Å/s, see conditions here | ~ 10-250 Å/s |
| Batch size |
|
|
|
|
|
|
| Allowed materials |
|
|
|
|
|
Base materials:
Seed metals:
|
| Comment |
|
|
|
* To deposit a cumulative thickness above 600 nm permission is required from metal@nanolab.dtu.dk to ensure enough material is present in the machine
** To deposit a cumulative thickness above 200 nm permission is required from metal@nanolab.dtu.dk to ensure enough material is present in the machine