Jump to content

Specific Process Knowledge/Thin film deposition/Deposition of Copper: Difference between revisions

Reet (talk | contribs)
m Deposition of Cu: added info on deposition rate
Reet (talk | contribs)
m Deposition of Cu: cluster sputter name
Line 12: Line 12:
! E-beam evaporation ([[Specific Process Knowledge/Thin film deposition/Temescal|Temescal]])
! E-beam evaporation ([[Specific Process Knowledge/Thin film deposition/Temescal|Temescal]])
! Sputter deposition ([[Specific Process Knowledge/Thin film deposition/Lesker|Lesker]])
! Sputter deposition ([[Specific Process Knowledge/Thin film deposition/Lesker|Lesker]])
! Sputter deposition ([[Specific Process Knowledge/Thin film deposition/Cluster-based_multi-chamber_high_vacuum_sputtering_deposition_system#Process_information|Cluster-based sputter system]])
! Sputter deposition ([[Specific Process Knowledge/Thin film deposition/Cluster-based multi-chamber high vacuum sputtering deposition system|Sputter-system Metal-Oxide (PC1) and Sputter-system Metal-Nitride (PC3)]])
|-  
|-  
|-style="background:WhiteSmoke; color:black"