Specific Process Knowledge/Thin film deposition/Deposition of Nickel: Difference between revisions

Reet (talk | contribs)
Reet (talk | contribs)
→Nickel deposition: added cluster sputterer
Line 126: Line 126:
* Photoresist  
* Photoresist  
* Metals  
* Metals  
|
*Almost any that do not outgas if you plan to use substrate heating. Check the cross-contamination sheets in Labmanager.
|
|
Base materials:<br>
Base materials:<br>
Line 148: Line 150:
|
|
|
|
|May use high-strength magnet for deposition
|Sample must be compatible with plating bath (pH = 3,65 and T = 52°C). Seed metal necessary.
|Sample must be compatible with plating bath (pH = 3,65 and T = 52°C). Seed metal necessary.
|-
|-
Line 153: Line 156:
|}
|}


'''*''' ''To deposit layers thicker than 600 nanometers permission is required from metal@danchip.dtu.dk to ensure enough material is present in the machine''
'''*''' ''To deposit layers thicker than 600 nanometers permission is required from metal@nanolab.dtu.dk to ensure enough material is present in the machine''