The materials manager is used for adding crystal structures and amorphous material parameters for use in data simulation. For most users the compounds are proberly of most interest, as it is in here that you can generate materials like In(x)Ga(1-x)As. I will add some of the basic material missing compared to the old software. | The materials manager is used for adding crystal structures and amorphous material parameters for use in data simulation. For most users the compounds are proberly of most interest, as it is in here that you can generate materials like In(x)Ga(1-x)As. I will add some of the basic material missing compared to the old software. | ||
For information about how to use the plugin | For information about how to use the plugin please look in section 3.2 in the manual opened by clicking on the ? in the software to right corner or from [http://labmanager.dtu.dk/view_binary.php?fileId=4246 LabManager]. | ||