For more info on these see the manual by clicking ? in the right panel for the plugin (Crystallite Size and Strain, Lattice Parameter Refinement, or %Crystallinity) or in [http://labmanager.dtu.dk/view_binary.php?fileId=4247 LabManager] | For more info on these see the manual by clicking ? in the right panel for the plugin (Crystallite Size and Strain, Lattice Parameter Refinement, or %Crystallinity) or in [http://labmanager.dtu.dk/view_binary.php?fileId=4247 LabManager] | ||
===Comprehensive Analysis/Lattice parameter refinement=== | ===Comprehensive Analysis/Lattice parameter refinement=== | ||
For Lattice parameter refinement, follow the steps for search and match. After phase identification do the following. | |||
*Configure lattice parameter refinement: | |||
**Select the dataset to analyse. | |||
**Select or deselect peaks that are to be used or not for the calculation. | |||
**Select the Angular correction to use. | |||
For more info on these see the manual by clicking ? in the right panel for the plugin (Crystallite Size and Strain, Lattice Parameter Refinement, or %Crystallinity) or in [http://labmanager.dtu.dk/view_binary.php?fileId=4247 LabManager] | For more info on these see the manual by clicking ? in the right panel for the plugin (Crystallite Size and Strain, Lattice Parameter Refinement, or %Crystallinity) or in [http://labmanager.dtu.dk/view_binary.php?fileId=4247 LabManager] | ||