Specific Process Knowledge/Characterization/XPS/NexsaOverview: Difference between revisions
Line 1: | Line 1: | ||
== Overview of the processing options on the XPS Nexsa== | == Overview of the processing options on the XPS Nexsa== | ||
The acquisition of an instrument like the Nexsa has to be done through a EU tender process. As a somewhat unexpected result of this process, we were offered the Nexsa at a very favorable price. We were therefore able to squeeze <span title="The only analytical option (that means excluded chillers, factory training courses, UPS etc) not chosen is a vacuum transfer module " > ''all'' </span> but one of the available options into the budget. That is, of course, very nice indeed, but we will have to investigate the applications of the various techniques as | The acquisition of an instrument like the Nexsa has to be done through a EU tender process. As a somewhat unexpected result of this process, we were offered the Nexsa at a very favorable price. We were therefore able to squeeze <span title="The only analytical option (that means excluded chillers, factory training courses, UPS etc) not chosen is a vacuum transfer module " > ''all'' </span> but one of the available options into the budget. That is, of course, very nice indeed, but it also means that we will have to investigate the applications of the various techniques as there is no applications waiting for a specific technique to become available. | ||
We have therefore compiled the table below that contains articles and application notes in which several of the available techniques are used | |||
The columns contain the following information (exclude are the columns where the content is evident): | |||
* '''Title''': Click on the title to access a pdf version of the article/application note. | |||
*'''Web of Science''': Click here to access the article in the Web of Science database (be sure to be logged in via DTU Inside in advance). This will enable you to browse the cited references and citations of the | |||
{| border="2" cellspacing="0" cellpadding="1" {{table}} | {| border="2" cellspacing="0" cellpadding="1" {{table}} |
Revision as of 11:15, 14 April 2020
Overview of the processing options on the XPS Nexsa
The acquisition of an instrument like the Nexsa has to be done through a EU tender process. As a somewhat unexpected result of this process, we were offered the Nexsa at a very favorable price. We were therefore able to squeeze all but one of the available options into the budget. That is, of course, very nice indeed, but it also means that we will have to investigate the applications of the various techniques as there is no applications waiting for a specific technique to become available.
We have therefore compiled the table below that contains articles and application notes in which several of the available techniques are used
The columns contain the following information (exclude are the columns where the content is evident):
- Title: Click on the title to access a pdf version of the article/application note.
- Web of Science: Click here to access the article in the Web of Science database (be sure to be logged in via DTU Inside in advance). This will enable you to browse the cited references and citations of the