Specific Process Knowledge/Characterization/XPS: Difference between revisions
| Line 80: | Line 80: | ||
|style="background:LightGrey; color:black"|Depth profiles | |style="background:LightGrey; color:black"|Depth profiles | ||
|style="background:WhiteSmoke; color:black"|Depth profiles with single Ar ion bombardment | |style="background:WhiteSmoke; color:black"|Depth profiles with single Ar ion bombardment | ||
* Monoatomic energy range 200- | * Monoatomic energy range 200-3000 eV | ||
|style="background:WhiteSmoke; color:black"|Depth profiles with MonoAtomic and Gas Cluster Ion Source ([[Media:MAGCIS.pdf |MAGCIS]]) | |style="background:WhiteSmoke; color:black"|Depth profiles with MonoAtomic and Gas Cluster Ion Source ([[Media:MAGCIS.pdf |MAGCIS]]) | ||
* Monoatomic energy range 200- | * Monoatomic energy range 200-4000 eV | ||
* Cluster mode energy range: 2-8 keV | * Cluster mode energy range: 2-8 keV | ||
*Cluster size range: 75-2000 atoms | *Cluster size range: 75-2000 atoms | ||
Revision as of 09:37, 14 April 2020
Feedback to this page: click here
The XPS tools at DTU Nanolab


In the basement under the cleanroom two X-ray Photoelectron Spectroscopy (XPS) systems are installed back-to-back in the center of room 904. They are both manufactured by Thermofisher and they enable the users to perform elemental and chemical analysis of samples. The XPS K-Alpha is a base technique instrument providing XPS analysis. The XPS Nexsa is an upgraded version with all options.
Elemental analysis
The XPS instrument enables elemental analysis, chemical state analysis on the sample surface or deeper down by a depth profiling. A comparison about techniques and instruments used for elemental analysis at DTU Nanolab can be found on the page Element analysis.
More about the different possibilities of the XPS instrument is found here:
Getting access to the XPS tools
Click HERE to see information on how to get access to the XPS.
Analyzing XPS spectra
The analysis of XPS spectra is an art in itself. Click on the link below to find a some examples in which the Avantage software package has been used to extract information from experiments.
Techniques and option on the XPS tools
| Equipment | K-Alpha | Nexsa | |
|---|---|---|---|
| Purpose | Main | XPS analysis using monochromated Al-Kα radiation at 1486.6 eV | XPS analysis using monochromated Al-Kα radiation at 1486.6 eV |
| Alternative/complementary |
| ||
| Performance | Spot size | XPS: 30µm - 400µm |
|
| Pass energy | 10-400 eV | 10-400 eV (XPS and ISS) | |
| Analysis modes | Scanned and snapshot | Scanned, snapshot and SnapMap | |
| Charge compensation | Flood gun to be used for charge compensation of non conductive samples only | Flood gun to be used for charge compensation of non conductive samples and for source of low energy electrons (REELS) | |
| Depth profiles | Depth profiles with single Ar ion bombardment
|
Depth profiles with MonoAtomic and Gas Cluster Ion Source (MAGCIS)
| |
| Substrates / Samples | Sample holder size | Maximum 60x60 mm | Maximum 60x60 mm |
| Sample height | Maximum 20 mm | Maximum 20 mm | |