Jump to content

Specific Process Knowledge/Characterization/XPS: Difference between revisions

Jmli (talk | contribs)
Jmli (talk | contribs)
Line 81: Line 81:
|style="background:WhiteSmoke; color:black"|Depth profiles with single Ar ion bombardment
|style="background:WhiteSmoke; color:black"|Depth profiles with single Ar ion bombardment
* Monoatomic energy range 200-3 keV
* Monoatomic energy range 200-3 keV
|style="background:WhiteSmoke; color:black"|Depth profiles with MonoAtomic and Gas Cluster Ion Source ([file:MAGCIS.pdf |MAGCIS])
|style="background:WhiteSmoke; color:black"|Depth profiles with MonoAtomic and Gas Cluster Ion Source ([[Media:MAGCIS.pdf |MAGCIS]])
* Monoatomic energy range 200-4 keV
* Monoatomic energy range 200-4 keV
* Cluster mode energy range: 2-8 keV
* Cluster mode energy range: 2-8 keV