Jump to content

Specific Process Knowledge/Etch/Etching of Silicon/Si etch using ASE: Difference between revisions

BGE (talk | contribs)
Jml (talk | contribs)
Line 46: Line 46:
! Process time  
! Process time  
| 5:56 mins
| 5:56 mins
! C<sub>4</sub>F<sub>4</sub> Flow
! C<sub>4</sub>F<sub>8</sub> Flow
| 0 sccm
| 0 sccm
| 120 sccm
| 120 sccm