Specific Process Knowledge/Thin film deposition/Deposition of Copper: Difference between revisions
Appearance
→Deposition of Cu: added the cluster sputterer |
|||
| Line 12: | Line 12: | ||
! E-beam evaporation ([[Specific Process Knowledge/Thin film deposition/Temescal|Temescal]]) | ! E-beam evaporation ([[Specific Process Knowledge/Thin film deposition/Temescal|Temescal]]) | ||
! Sputter deposition ([[Specific Process Knowledge/Thin film deposition/Lesker|Lesker]]) | ! Sputter deposition ([[Specific Process Knowledge/Thin film deposition/Lesker|Lesker]]) | ||
! Sputter deposition ([[Specific Process Knowledge/Thin film deposition/Cluster-based_multi-chamber_high_vacuum_sputtering_deposition_system#Process_information|Cluster-based sputter system]]) | |||
|- | |- | ||
|-style="background:WhiteSmoke; color:black" | |-style="background:WhiteSmoke; color:black" | ||
| Line 19: | Line 20: | ||
|Sputter deposition of Cu | |Sputter deposition of Cu | ||
(not line-of-sight deposition) | (not line-of-sight deposition) | ||
|Sputter deposition of Cu | |||
(not line-of-sight deposition) | |||
|- | |- | ||
| Line 26: | Line 28: | ||
!Pre-clean | !Pre-clean | ||
|Ar ion bombardment | |Ar ion bombardment | ||
|RF Ar clean | |||
|RF Ar clean | |RF Ar clean | ||
| Line 33: | Line 36: | ||
!Layer thickness | !Layer thickness | ||
|10Å to 1µm* | |10Å to 1µm* | ||
|10Å to 1µm** | |||
|10Å to 1µm** | |10Å to 1µm** | ||
| Line 41: | Line 45: | ||
|1Å/s to 10Å/s | |1Å/s to 10Å/s | ||
| ~1Å/s | | ~1Å/s | ||
| depends on process parameters | |||
|- | |- | ||
| Line 52: | Line 57: | ||
*smaller pieces | *smaller pieces | ||
*Up to 1x6" wafers | *Up to 1x6" wafers | ||
| | |||
*Up to 10x4" or 6" wafers | |||
*or many smaller pieces | |||
|- | |- | ||
| Line 76: | Line 84: | ||
* SU-8 | * SU-8 | ||
* Metals | * Metals | ||
| | |||
*Almost any as long as they do not outgas if you are planning to heat the substrate. Check the cross-contamination sheets in Labmanager. | |||
|-style="background:WhiteSmoke; color:black" | |-style="background:WhiteSmoke; color:black" | ||
! Comment | ! Comment | ||
|As of March 2020, Cu has not yet been deposited in this machine. | |As of March 2020, Cu has not yet been deposited in this machine. | ||
Please contact the Thin Film group to develop a process. | Please contact the Thin Film group to develop a process. | ||
| | |||
| | | | ||
|} | |} | ||
''' | '''*''' ''To deposit layers thicker than 600 nm permission is required to ensure that there is enough metal (contact metal@nanolab.dtu.dk)'' | ||
'''*''' ''To deposit layers thicker than 200 nm permission is required to ensure that there is enough metal (contact metal@nanolab.dtu.dk)'' | '''**''' ''To deposit layers thicker than 200 nm permission is required to ensure that there is enough metal (contact metal@nanolab.dtu.dk)'' | ||
==Studies of Cu deposition== | ==Studies of Cu deposition== | ||