== 1,2: Protective Pt deposition == | == 1,2: Protective Pt deposition == | ||
[[File:fig1.PNG| | [[File:fig1.PNG|600px]] | ||
Fig 1: Sketch of electron beam Pt deposition. | Fig 1: Sketch of electron beam Pt deposition. | ||
[[File:fig2. | [[File:fig2.PNG|600px]] | ||
Fig 2: Sketch of subsequent platinum deposition. | Fig 2: Sketch of subsequent platinum deposition. | ||
[[File:fig3_1.tif]][[File:fig3_2.tif]] | [[File:fig3_1.tif]][[File:fig3_2.tif]] | ||
Fig 3: SE images acquired before and after electron beam deposited platinum. | Fig 3: SE images acquired before and after electron beam deposited platinum. | ||