New page: == Clean with: == *RCA - ''two step process to remove organics and metals'' *7-up - ''piranha etch of wafers and masks - removes organiscs and alkali ions'' *BHF - ''etching of predep gla...
 
No edit summary
Line 4: Line 4:
*7-up - ''piranha etch of wafers and masks - removes organiscs and alkali ions''
*7-up - ''piranha etch of wafers and masks - removes organiscs and alkali ions''
*BHF - ''etching of predep glass''
*BHF - ''etching of predep glass''
*Polisher - ''Grammophone polisher for mechanical clean of glass wafers''

Revision as of 14:35, 4 October 2007

Clean with:

  • RCA - two step process to remove organics and metals
  • 7-up - piranha etch of wafers and masks - removes organiscs and alkali ions
  • BHF - etching of predep glass