'''Feedback to this page''': '''[mailto:labadviser@nanolab.dtu.dk?Subject=Feed%20back%20from%20page%20http://labadviser.nanolab.dtu.dk/index.php/Specific_Process_Knowledge/Thin_film_deposition/Deposition_of_NiFe click here]''' | '''Feedback to this page''': '''[mailto:labadviser@nanolab.dtu.dk?Subject=Feed%20back%20from%20page%20http://labadviser.nanolab.dtu.dk/index.php/Specific_Process_Knowledge/Thin_film_deposition/Deposition_of_NiFe click here]''' | ||
== | ==Deposition of Nickel Iron alloy== | ||
Nickel Iron has been sputter deposited in the [[Specific_Process_Knowledge/Thin_film_deposition/Lesker|Sputter-system (Lesker)]] here at Nanolab. | Nickel Iron has previously been sputter deposited in the [[Specific_Process_Knowledge/Thin_film_deposition/Lesker|Sputter-system (Lesker)]] here at Nanolab. | ||
Read more about process parameters and previous results of sputtering Ni-Fe in the Lesker sputter system [[/Sputtering of NiFe in the Lesker sputter system|here]]. | Read more about process parameters and previous results of sputtering Ni-Fe in the Lesker sputter system [[/Sputtering of NiFe in the Lesker sputter system|here]]. | ||
Revision as of 13:53, 24 March 2020
Feedback to this page: click here
Deposition of Nickel Iron alloy
Nickel Iron has previously been sputter deposited in the Sputter-system (Lesker) here at Nanolab.
Read more about process parameters and previous results of sputtering Ni-Fe in the Lesker sputter system here.