'''Feedback to this page''': '''[mailto:LabAdviser@nanolab.dtu.dk?Subject=Feed%20back%20from%20page%20http://labadviser.nanolab.dtu.dk/index.php/Specific_Process_Knowledge/Thin_film_deposition/Deposition_of_Copper click here]'''
'''Feedback to this page''': '''[mailto:LabAdviser@nanolab.dtu.dk?Subject=Feed%20back%20from%20page%20http://labadviser.nanolab.dtu.dk/index.php/Specific_Process_Knowledge/Thin_film_deposition/Deposition_of_Copper click here]'''


== Deposition of Cu ==
= Deposition of Cu =
Copper can be deposited by e-beam evaporation or sputtering at Nanolab. In the chart below you can compare the different deposition equipment.
Copper can be deposited by e-beam evaporation or sputtering at Nanolab. In the chart below you can compare the different deposition equipment.


Line 91: Line 91:


[[/Deposition of Copper|Roughness of Cu layers]] - ''Roughness of Cu layers deposited with the Alcatel e-beam evaporator''
[[/Deposition of Copper|Roughness of Cu layers]] - ''Roughness of Cu layers deposited with the Alcatel e-beam evaporator''
[[Specific_Process_Knowledge/Thin_film_deposition/Lesker/Stress_dependence_on_sputter_parameters_in_the_Lesker_sputter_system#Cu:_Low_stress|Stress in sputtered Cu]] - ''Low stress in Cu films sputtered with the Sputter-System (Lesker)'']]

Revision as of 14:17, 26 March 2020

Feedback to this page: click here

Deposition of Cu

Copper can be deposited by e-beam evaporation or sputtering at Nanolab. In the chart below you can compare the different deposition equipment.


E-beam evaporation (Temescal) Sputter deposition (Lesker)
General description E-beam deposition of Cu

(line-of-sight deposition)

Sputter deposition of Cu

(not line-of-sight deposition)

Pre-clean Ar ion bombardment RF Ar clean
Layer thickness 10Å to 1µm* 10Å to 1µm**
Deposition rate 1Å/s to 10Å/s ~1Å/s
Batch size
  • Up to 4x6" wafers
  • Up to 3x8" wafers (ask for holder)
  • smaller pieces
  • smaller pieces
  • Up to 1x6" wafers
Allowed materials
  • Silicon
  • Silicon oxide
  • Silicon (oxy)nitride
  • Photoresist
  • PMMA
  • Mylar
  • SU-8
  • Metals
Comment As of March 2020, Cu has not yet been deposited in this machine.

Please contact the Thin Film group to develop a process.

** To deposit layers thicker than 600 nm permission is required to ensure that there is enough metal (contact metal@nanolab.dtu.dk)

* To deposit layers thicker than 200 nm permission is required to ensure that there is enough metal (contact metal@nanolab.dtu.dk)

Studies of Cu deposition processes

Roughness of Cu layers - Roughness of Cu layers deposited with the Alcatel e-beam evaporator Stress in sputtered Cu - Low stress in Cu films sputtered with the Sputter-System (Lesker)]]