Procedure of ultra-sectionning in images: | Procedure of ultra-sectionning in images: | ||
[[File:1.jpg|400px|left|thumb|Trimming resin block using diamond knife]]<br /> | [[File:1.jpg|400px|left|thumb|1. Trimming resin block using diamond knife]]<br /> | ||
[[File:8 (2).jpg|400px|left|thumb|2. Ultra-sectionning of sample using diamond knife with water boat]]<br /> | |||