==''Proposed | ==''Proposed'' quality control (QC) procedure for the Thermal evaporator== | ||
{| border="1" cellspacing="2" cellpadding="2" colspan="3" | {| border="1" cellspacing="2" cellpadding="2" colspan="3" | ||
| Line 144: | Line 144: | ||
|} | |} | ||
Thicknesses are measured in 5 points with one of the Dektak instruments. <br> | Thicknesses are measured in 5 points with one of the Dektak instruments. <br> | ||
Additionally we monitor the state of the Al crucible and ensure that it does not contain enough Al for it to wet the outside and short circuit the heater. | |||
|} | |} | ||