| Line 138: | Line 138: | ||
Using the Picoscope is straightforward. The Start/Stop recording buttons are located in the lower left corner of the GUI; the recording has to be done manually. Below is a typical screen dump of the GUI from a process run. | Using the Picoscope is straightforward. The Start/Stop recording buttons are located in the lower left corner of the GUI; the recording has to be done manually. Below is a typical screen dump of the GUI from a process run. | ||
[[image:Picodump2.png|800px]] | [[image:Picodump2.png|800px]] | ||
One can adjust several parameters: | One can adjust several parameters: | ||
* Collection time: Here, it is 5 seconds per division, can also be 10 seconds per division | * Collection time: Here, it is 5 seconds per division, can also be 10 seconds per division | ||