==Sputtering of TiW==


Deposition of TiW alloy can be done in the Wordentec. If necessary, processes may also be developed for depositing TiW in the Lesker sputter setups (contact responsible staff for this).
Deposition of TiW alloy can be done in the [[Specific Process Knowledge/Thin film deposition/Wordentec|Wordentec]]. If necessary, processes may also be developed for depositing TiW in the Lesker sputter setups (contact responsible staff for this).
 
 
 
==Sputtering of TiW==


* [[/Sputtering of TiW in Wordentec|Sputtering of TiW in Wordentec]]
* [[/Sputtering of TiW in Wordentec|Sputtering of TiW in Wordentec]]





Revision as of 13:43, 19 March 2020

Feedback to this page: click here

Sputtering of TiW

Deposition of TiW alloy can be done in the Wordentec. If necessary, processes may also be developed for depositing TiW in the Lesker sputter setups (contact responsible staff for this).


Sputter deposition (Wordentec)
General description Sputter deposition of TiW
Pre-clean RF Ar clean
Layer thickness .
Deposition rate Depending on process parameters, see here.
Batch size
  • 24x2" wafers or
  • 6x4" wafers or
  • 6x6" wafers
Allowed substrates
  • Silicon wafers
  • Quartz wafers
  • Pyrex wafers
Allowed materials
  • Silicon oxide
  • Silicon (oxy)nitride
  • Photoresist
  • PMMA
  • Mylar
  • SU-8
  • Metals
Comments TiW alloy: 10%/90% by weight