Process optimization using the Picoscope
The Pegasus tools were delivered with a set of standard recipes
- 4 cycles of Process A
-
Recorded with the SPTS software
-
Recorded with the Picoscope
- 4 cycles of Process D4
-
Recorded with the SPTS software
-
Recorded with the Picoscope