*'''(1402) DCH 100mm M35G 750nm''' Dispense 1ml@1000rpm; spin-off 60s@5000rpm; softbake 90s@130°C
*'''(1402) DCH 100mm M35G 750nm''' Dispense 1ml@1000rpm; spin-off 60s@5000rpm; softbake 90s@130°C
*'''(1403) DCH 150mm M35G 1000nm''' Dispense 3ml@1000rpm; spin-off 60s@2630rpm; softbake 90s@130°C
*'''(1403) DCH 150mm M35G 1000nm''' Dispense 3ml@1000rpm; spin-off 60s@2630rpm; softbake 90s@130°C
*'''(1404) DCH 100mm M35G 1000nm''' Dispense 1ml@1000rpm; spin-off 60s@26300rpm; softbake 90s@130°C
*'''(1404) DCH 100mm M35G 1000nm''' Dispense 1ml@1000rpm; spin-off 60s@2630rpm; softbake 90s@130°C
*'''(1405) DCH 150mm M35G 1400nm''' Dispense 3ml@1000rpm; spin-off 60s@1310rpm; softbake 90s@130°C
*'''(1405) DCH 150mm M35G 1400nm''' Dispense 3ml@1000rpm; spin-off 60s@1310rpm; softbake 90s@130°C
*'''(1406) DCH 100mm M35G 1400nm''' Dispense 1ml@1000rpm; spin-off 60s@1310rpm; softbake 90s@130°C
*'''(1406) DCH 100mm M35G 1400nm''' Dispense 1ml@1000rpm; spin-off 60s@1310rpm; softbake 90s@130°C