Specific Process Knowledge/Lithography/Aligners/Aligner: Maskless 03 processing: Difference between revisions
Appearance
| Line 102: | Line 102: | ||
==Writing speed== | ==Writing speed== | ||
According to specs, the writing speed of Aligner: Maskless 03 is 1100mm<sup>2</sup>/min in fast mode. Using the high quality exposure mode cuts this speed in half, to approximately 550mm<sup>2</sup>/min. The writing speed for a 100x100mm<sup>2</sup> area measured during installation of the machine (acceptance test) was ~1200mm<sup>2</sup>/min. | According to specs, the writing speed of Aligner: Maskless 03 is 1100mm<sup>2</sup>/min in fast mode. Using the high quality exposure mode cuts this speed in half, to approximately 550mm<sup>2</sup>/min. The writing speed for a 100x100mm<sup>2</sup> area measured during installation of the machine (acceptance test) was ~1200mm<sup>2</sup>/min. | ||
'''Speed vs. area:''' | '''Speed vs. area:''' | ||