==Acceptance test== | ==Acceptance test== | ||
Acceptance criteria on a 100 X 100 mm<sup>2</sup> area: Width of smallest resolved line | Acceptance criteria on a 100 X 100 mm<sup>2</sup> area: Width of smallest resolved line 1000±120 nm (quality), alignment error 500 nm (quality), writing speed 1100 mm<sup>2</sup>/min (fast). | ||
The acceptance test also included a verification of back side alignment (better than 1 µm), as well as a test of the conversion speed (less than 15 minutes for a dense design of circles). | The acceptance test also included a verification of back side alignment (better than 1 µm), as well as a test of the conversion speed (less than 15 minutes for a dense design of circles). | ||
| Line 116: | Line 116: | ||
|- | |- | ||
|-style="background:silver; color:black" | |-style="background:silver; color:black" | ||
!colspan="2"| | !colspan="2"| | ||
!Width of smallest resolved line [nm] | !Width of smallest resolved line [nm] | ||
!Alignment error (TSA) [nm] | !Alignment error (TSA) [nm] | ||
| Line 124: | Line 124: | ||
|- | |- | ||
|-style="background:WhiteSmoke; color:black" | |-style="background:WhiteSmoke; color:black" | ||
|rowspan="2"| | |rowspan="2"|FAT December 2019 | ||
|'''X''' | |'''X''' | ||
| | | 985±72 | ||
| | | 427 | ||
|rowspan="2" align="mid"| | |rowspan="2" align="mid"| 1269 | ||
|- | |- | ||
|-style="background:WhiteSmoke; color:black" | |-style="background:WhiteSmoke; color:black" | ||
|'''Y''' | |'''Y''' | ||
| | | 953±47 | ||
| | | 362 | ||
|- | |- | ||
|-style="background:WhiteSmoke; color:black" | |-style="background:WhiteSmoke; color:black" | ||
| | |SAT February 2020 | ||
| | | | ||
| | | ≤1000 | ||
| | | ≤500 | ||
| | | align="mid"| 1212 | ||
|} | |} | ||