*Temperatures close to the glass transition temperature of the polymer give the best results when it comes to pattern replication. | *Temperatures close to the glass transition temperature of the polymer give the best results when it comes to pattern replication. | ||
*Temperatures that are 5 degrees above the glass transition | *Temperatures that are 5 degrees above the glass transition temperature of the polymer give the best results when bonding lids on top of chips. If bonding chip to lid, where the polymers are of different types/grades this rule will not apply | ||
|- | |- | ||