Jump to content

Specific Process Knowledge/Lithography/Baking: Difference between revisions

Elkh (talk | contribs)
Elkh (talk | contribs)
Line 217: Line 217:
In order to avoid thermal curing of SU-8 residues on the hotplates, they are temperature limited to 110°C.
In order to avoid thermal curing of SU-8 residues on the hotplates, they are temperature limited to 110°C.


'''The user manual, and contact information can be found in LabManager: [http://labmanager.danchip.dtu.dk/function.php?module=Machine&view=view&mach=122 Hotplate 1 (SU8)] [http://labmanager.danchip.dtu.dk/function.php?module=Machine&view=view&mach=124 Hotplate 2 (SU8)]'''
'''The user manual, and contact information can be found in LabManager: [http://labmanager.danchip.dtu.dk/function.php?module=Machine&view=view&mach=122 Hotplate 1 (SU8)] [http://labmanager.danchip.dtu.dk/function.php?module=Machine&view=view&mach=124 Hotplate 2 (SU8)] [http://labmanager.danchip.dtu.dk/function.php?module=Machine&view=view&mach=169 Hotplate 3 (SU8)] [http://labmanager.danchip.dtu.dk/function.php?module=Machine&view=view&mach=169 Hotplate 4 (SU8)]'''
<br clear="all" />
<br clear="all" />