Specific Process Knowledge/Lithography/EBeamLithography/High resolution patterning with HSQ: Difference between revisions
Appearance
No edit summary |
No edit summary |
||
| Line 15: | Line 15: | ||
In most cases the time from taking HSQ out of the fridge to spin coat, and between spin coat and exposure as well as the time between exposure and development impacts on the resolution achieved. | In most cases the time from taking HSQ out of the fridge to spin coat, and between spin coat and exposure as well as the time between exposure and development impacts on the resolution achieved. | ||
It is therefore not recommended to use HSQ as a trainings resist. | It is therefore not recommended to use HSQ as a trainings resist. | ||
/BR | /BR | ||
The details of the process is shown below in the table: | The details of the process is shown below in the table: | ||