Jump to content

Specific Process Knowledge/Imprinting: Difference between revisions

Elkh (talk | contribs)
Elkh (talk | contribs)
Line 12: Line 12:


A stamp for imprint lithography is usually made in Si or SiO, however other materials could also be used.
A stamp for imprint lithography is usually made in Si or SiO, however other materials could also be used.
Here is a process flow for stamp made of SU8 resist.[[media:Imrinting_layer_spinning.docx‎ |Preparation substrate‎ with imprint layer]]
Here is a process flow for stamp made of SU8 resist.[[media:Stamp_Fabrication.docx‎ |Stamp fabrication]]


==Imprint resist==
==Imprint resist==