Specific Process Knowledge/Etch/KOH Etch: Difference between revisions
Appearance
| Line 147: | Line 147: | ||
|style="background:WhiteSmoke; color:black"| | |style="background:WhiteSmoke; color:black"| | ||
*Mixing ratios giving 28 wt% KOH solutions | *Mixing ratios giving 28 wt% KOH solutions | ||
KOH:H<sub>2</sub>O - 1000 ml: 1200 ml, when using premixed 50% KOH solution | KOH:H<sub>2</sub>O - 1000 ml: 1200 ml, when using premixed 50% KOH solution | ||
|style="background:WhiteSmoke; color:black"| | |style="background:WhiteSmoke; color:black"| | ||