A 2µm nLOF resist film is fully developed in 20-30s using TMAH (AZ 726 MIF). However, the development can be continued to 60s in order to get a nore negative resist profile (increase the under-cut).
A 2µm nLOF resist film is fully developed in 20-30s using TMAH (AZ 726 MIF). However, the development can be continued to 60s in order to get a more negative resist profile (increase the under-cut).