Line 74: Line 74:


It was tried(jan09) to lift 2,5µ Al on 4,2µ negative resist on top of 11µ Apox SiO2 in acetone sonic-bath.
It was tried(jan09) to lift 2,5µ Al on 4,2µ negative resist on top of 11µ Apox SiO2 in acetone sonic-bath.
This process was done by steps evaporating only 5000Å a time with 5min pause and pressure down to at least 2E-6.
This process was done in steps evaporating 5000Å a time with 5min pause and pressure down to at least 2E-6.