Specific Process Knowledge/Thermal Process/C2 Furnace III-V oxidation: Difference between revisions
| Line 19: | Line 19: | ||
==Process knowledge== | ==Process knowledge== | ||
*[[Specific_Process_Knowledge/Thermal_Process/Oxidation/Oxidation_on_III- | *[[Specific_Process_Knowledge/Thermal_Process/Oxidation/Oxidation_on_III-V_oxidation_furnace_(C2)|Standard wet oxidation recipe on the III-V oxidation furnace]] | ||
==Overview of the performance of the III-V Oven and some process related parameters== | ==Overview of the performance of the III-V Oven and some process related parameters== | ||
Revision as of 07:39, 15 August 2019
THIS PAGE IS UNDER CONSTRUCTION
Feedback to this page: click here
III-V Oxidation furnace (C2)
The III-V Oxidaiont furnace (C2) is being use on August 2019 for wet thermal oxidation of III-V devices instead of the III-V ovn, for instance for lateral oxidation of thin AlGaAs layers to defined apertures in light-limiting diodes.
The furnace is an old Tempress horizontal furnace. The quartz boat is loaded manually into the furnace by use of a push rod. The furnace is cooled down to room temperature when it is not being used.
Before use, devices have to be cleaned. A short BHF dip can be used to remove any native oxide which can be difficult to penetrate by a wet thermal oxidation.
Please check the cross contamination information in LabManager before you use the furnace.
The user manual and contact information can be found in LabManager:
Process knowledge
| Purpose |
| |
|---|---|---|
| Performance | Lateral oxidation rate |
|
| Process parameter range | Process temperature |
|
| Process pressure |
| |
| Gasses on the system |
| |
| Substrates | Batch size |
|
| Substrate materials allowed |
|