Specific Process Knowledge/Characterization/Four-Point Probe: Difference between revisions
| Line 23: | Line 23: | ||
Sheet Resistivity = Sheet Resistance = Surface Resistivity = Surface Resistance | Sheet Resistivity = Sheet Resistance = Surface Resistivity = Surface Resistance | ||
'''Limits of Measurement Capability''' | |||
1. The material must be capable of being probed, i.e. the probes must be able to make ohmic contact with the material e.g. Germanium, Silicon and metals. Materials such as Gallium Arsenide cannot normally be probed unless it is doped and measured with special measuring techniques such as that in the Four Dimensions Inc. GaAs probe. | 1. The material must be capable of being probed, i.e. the probes must be able to make ohmic contact with the material e.g. Germanium, Silicon and metals. Materials such as Gallium Arsenide cannot normally be probed unless it is doped and measured with special measuring techniques such as that in the Four Dimensions Inc. GaAs probe. | ||
2. Very low resistivity material e.g. aluminum, gold, platinum may require the maximum current from the current source to achieve a reading on the digital voltage display. Only very thin films from 10’s nm up to 1 micron thickness can be measured. Sample with expected sheet resistance less than 1 ohm/square may not possible to measure. | 2. Very low resistivity material e.g. aluminum, gold, platinum may require the maximum current from the current source to achieve a reading on the digital voltage display. Only very thin films from 10’s nm up to 1 micron thickness can be measured. Sample with expected sheet resistance less than 1 ohm/square may not possible to measure. | ||
3. High resistivity material e.g. ion-implanted Silicon wafer, silicon on sapphire, can be measured using very low current (about 1uA or less) and trying to avoid a greater voltage indication than 200mV. Probably sheet resistance up to 107 ohms/square can be measured. | 3. High resistivity material e.g. ion-implanted Silicon wafer, silicon on sapphire, can be measured using very low current (about 1uA or less) and trying to avoid a greater voltage indication than 200mV. Probably sheet resistance up to 107 ohms/square can be measured. | ||
4. Low measurement result could be from electrical noise due to poor contact condition, thermally induced voltages, actinic effects, offset voltages produced by the devices in the current source etc. | 4. Low measurement result could be from electrical noise due to poor contact condition, thermally induced voltages, actinic effects, offset voltages produced by the devices in the current source etc. | ||
Revision as of 11:18, 8 August 2019
Feedback to this page: click here
Four-Point Probe
The set-up of the four point probe is four the tungsten carbide electrodes/probes.The power source (DC) sends a current through the two outer electrodes. A digital voltage meter (DVM) measures the potential drop between the two inner electrodes.
The sheet resistance can then be calculated using the equation below:
This equation is only valid if: i) the material being tested is no thicker than 40% of the spacing between the probes, and ii) the lateral size of the sample is sufficiently large. If this is not the case, then geometric correction factors are needed to account for the size, shape, and thickness of the sample.
Bulk resistivity for wafers and films = sheet resistance x wafer thickness in cm (Unit ohm.cm)
Bulk resistivity for a semi-infinite volume = 2 x π x S x V/I where is S is the probe spacing in cm (Unit ohm.cm)
A sample is usually defined as a “semi-infinite volume” if it extends to infinity in all directions below a plane on which four probes are located.
Note:
Volume Resistivity = Volume Resistance = Bulk Resistivity = Bulk Resistance
Sheet Resistivity = Sheet Resistance = Surface Resistivity = Surface Resistance
Limits of Measurement Capability
1. The material must be capable of being probed, i.e. the probes must be able to make ohmic contact with the material e.g. Germanium, Silicon and metals. Materials such as Gallium Arsenide cannot normally be probed unless it is doped and measured with special measuring techniques such as that in the Four Dimensions Inc. GaAs probe.
2. Very low resistivity material e.g. aluminum, gold, platinum may require the maximum current from the current source to achieve a reading on the digital voltage display. Only very thin films from 10’s nm up to 1 micron thickness can be measured. Sample with expected sheet resistance less than 1 ohm/square may not possible to measure.
3. High resistivity material e.g. ion-implanted Silicon wafer, silicon on sapphire, can be measured using very low current (about 1uA or less) and trying to avoid a greater voltage indication than 200mV. Probably sheet resistance up to 107 ohms/square can be measured.
4. Low measurement result could be from electrical noise due to poor contact condition, thermally induced voltages, actinic effects, offset voltages produced by the devices in the current source etc.
There are two four point probes at Nanolab. Four point probe from Jandel is located inside the cleanroom(D-3) and Four-Point Probe from Veeco is now located in the basement(346-904).
Four-Point Probe from Jandel
The Four point probe is manufactured by Jandel Engineering Limited and using Jandel probe head and the RM3000+ Test Unit which can supply constant current between 10nA and 99.99mA, and measure voltage from 0.01mV to 1250mV.
For sheet resistance measurements, the quoted range is 1 milliohm/square to 5x108 ohms/square. Measurements outside this range are possible but with possible reduced accuracy. For volume (bulk) resistivity measurements, the quoted range is 1 milliohm.cm to 1x106 ohm.cm. Measurements outside of this range may be possible but will depend on sample type e.g. whether the sample is a thin layer.
Multiposition Probe stand can measure on wafers up to 200mm diameter. The Θ movement clicks in four positions at 90 degrees and the linear movement in up to 10 positions giving repeat placement accuracy of +/- 1mm.
Four-Point Probe from Veeco
The Four-Point Probe is a Veeco FPP-5000 for I/V measurement. The main purpose is to measure resistance and resistivity on a 4" silicon wafer. But can also be used to find thickness of thin layers or test if is a N- or P-type wafer.

It works only for 4" wafers because a special holder is need.
The user manual, technical information and contact information can be found in LabManager:
| Purpose | Resistance and resistivity measurement | |
|---|---|---|
| Process parameter range | Process Temperature |
|
| Process pressure |
| |
| Substrates | Batch size |
|
| Substrate material allowed |
|