There are two four point probes at Nanolab. Four point probe from Jandel is located inside the cleanroom(D-3) and Four-Point Probe from Veeco is now located in the basement(346-904). | There are two four point probes at Nanolab. Four point probe from Jandel is located inside the cleanroom(D-3) and Four-Point Probe from Veeco is now located in the basement(346-904). | ||
==Four-Point Probe from Jandel== | |||
[[Image:Jandel_four_point_probe.PNG |thumb|400x400px|Four point probe: positioned in cleanroom D-3]] | [[Image:Jandel_four_point_probe.PNG |thumb|400x400px|Four point probe: positioned in cleanroom D-3]] | ||
Line 22: | Line 24: | ||
==Four-Point Probe from Veeco== | |||
The Four-Point Probe is a Veeco FPP-5000 for I/V measurement. The main purpose is to measure resistance and resistivity on a 4" silicon wafer. But can also be used to find thickness of thin layers or test if is a N- or P-type wafer. [[Image:4pointprobe.jpg|thumb|300x300px|Four point probe: positioned in 346-904]] | |||
It works only for 4" wafers because a special holder is need. | |||
'''The user manual, technical information and contact information can be found in LabManager:''' | '''The user manual, technical information and contact information can be found in LabManager:''' |
Revision as of 13:37, 7 August 2019
Four-Point Probe
Feedback to this page: click here
There are two four point probes at Nanolab. Four point probe from Jandel is located inside the cleanroom(D-3) and Four-Point Probe from Veeco is now located in the basement(346-904).
Four-Point Probe from Jandel
The Four point probe is manufactured by Jandel Engineering Limited and using Jandel probe head and the RM3000+ Test Unit which can supply constant current between 10nA and 99.99mA, and measure voltage from 0.01mV to 1250mV.
For sheet resistance measurements, the quoted range is 1 milliohm/square to 5x108 ohms/square. Measurements outside this range are possible but with possible reduced accuracy. For volume (bulk) resistivity measurements, the quoted range is 1 milliohm.cm to 1x106 ohm.cm. Measurements outside of this range may be possible but will depend on sample type e.g. whether the sample is a thin layer.
Multiposition Probe stand can measure on wafers up to 200mm diameter. The Θ movement clicks in four positions at 90 degrees and the linear movement in up to 10 positions giving repeat placement accuracy of +/- 1mm.
Four-Point Probe from Veeco
The Four-Point Probe is a Veeco FPP-5000 for I/V measurement. The main purpose is to measure resistance and resistivity on a 4" silicon wafer. But can also be used to find thickness of thin layers or test if is a N- or P-type wafer.
It works only for 4" wafers because a special holder is need.
The user manual, technical information and contact information can be found in LabManager:
Purpose | Resistance and resistivity measurement | |
---|---|---|
Process parameter range | Process Temperature |
|
Process pressure |
| |
Substrates | Batch size |
|