I (bghe@nanolab) tried with two different gas regimes: CF4 and C4F8. I only made a few tests with CF4 since I got a very bad selectivity to the resist mask and I dicided to go for the C4F8 instead.<br>
I (bghe@nanolab 2016) tried with two different gas regimes: CF4 and C4F8. I only made a few tests with CF4 since I got a very bad selectivity to the resist mask and I dicided to go for the C4F8 instead.<br>
Zhibo Li @ Danchip has also tried (December 2016) with similar setting, see his results in this file: [[:File:Zhibo Li SiO2 ICP etch (dose205).docx]]