| [[Image:DREM2pic1.jpg |frame|x300px|200nm trenches etched with 100 cycles (cross section view)]]
| [[Image:DREM2pic1.jpg |frame|x300px|200nm trenches etched with 100 cycles (cross section view)]]
| [[Image:DREM1pic2.jpg |frame|x300px|200nm pillars etched with 100 cycles (cross section view)]]
| [[Image:DREM2pic2.jpg |frame|x300px|200nm pillars etched with 100 cycles (cross section view)]]
| [[Image:DREM1pic3.jpg |frame|x300px|200nm pillars etched with 100 cycles (tilted view)]]
| [[Image:DREM2pic3.jpg |frame|x300px|200nm pillars etched with 100 cycles (tilted view)]]
| [[Image:DREM2pic4.jpg |frame|x300px|Pillars etched with 100 cycles, patterns defined with EBL and ZEP resist, smallest dimesion of 100nm (tilted view)]]
|}
|}