Below are some etched silicon nanostructures with the recipe '''DREM 1kW nano''' | Below are some etched silicon nanostructures with the recipe '''DREM 1kW nano''' | ||
{| | {| | ||
| [[Image:DREM1pic1.jpg |frame | | [[Image:DREM1pic1.jpg |frame|x300px|200nm trenches etched with 125 cycles (cross section view)]] | ||
| [[Image:DREM1pic2.jpg |frame|x300px|200nm pillars etched with 100 cycles | | [[Image:DREM1pic2.jpg |frame|x300px|200nm pillars etched with 100 cycles (cross section view)]] | ||
| [[Image:DREM1pic3.jpg |frame|x300px|200nm pillars etched with 100 cycles | | [[Image:DREM1pic3.jpg |frame|x300px|200nm pillars etched with 100 cycles (tilted view)]] | ||
|} | |} | ||
Below are some etched silicon nanostructures with the recipe '''DREM 0.5kW nano''' | Below are some etched silicon nanostructures with the recipe '''DREM 0.5kW nano''' | ||