Specific Process Knowledge/Etch/DRIE-Pegasus/showerheadchange/polySi/Cpoly4: Difference between revisions
Jump to navigation
Jump to search
No edit summary |
No edit summary |
||
Line 23: | Line 23: | ||
| Pegasus/jmli | | Pegasus/jmli | ||
| 10 minute TDESC clean + 45 sec barc etch | | 10 minute TDESC clean + 45 sec barc etch | ||
| | | nanolab/jml/showerhead/Cpoly4, 20 cycles or 2:16 minutes | ||
| S004733 | | S004733 | ||
| New showerhead | | New showerhead |
Revision as of 22:21, 25 November 2019
Date | Substrate Information | Process Information | SEM Images | ||||||
---|---|---|---|---|---|---|---|---|---|
Wafer info | Mask | Material/ Exposed area | Tool / Operator | Conditioning | Recipe | Wafer ID | Comments | ||
3/12-2014 | 1/4 6" Wafer with 210 nm oxide and 1800 nm polysilicon CB on oxide carrier | standard stepper mask (50 nm barc + 320 nm krf) | Si / 50+ % | Pegasus/jmli | 10 minute TDESC clean + 45 sec barc etch | nanolab/jml/showerhead/Cpoly4, 20 cycles or 2:16 minutes | S004733 | New showerhead |