* 1064nm, F255mm: 41 W
* 1064nm, F255mm: 41 W
|}
|}
[[media:AvgPower_1064nm_F255mm.png|1064nm, F255nm Avg. output power]]
* [[media:AvgPower_1064nm_F255mm.png|Graph 1064nm, F255nm Avg. output power]]