|style="background:LightGrey; color:black"|Max. output power @100%(laser TB width – picosecond)  
|style="background:LightGrey; color:black"|Max. output power @100%(laser TB width – picosecond)  
|style="background:WhiteSmoke; color:black"|
|style="background:WhiteSmoke; color:black"|
{| {{table}}
{| {{table}}
Line 98: Line 97:
* 532nm, F255mm: not measured
* 532nm, F255mm: not measured
* 1064nm, F255mm: 41 W
* 1064nm, F255mm: 41 W
|}
[[media:AvgPower_1064nm_F255mm.png|1064nm, F255nm Avg. output power]]


|}
|}
|}
|-
|-