Specific Process Knowledge/Characterization/XPS/Processing/ALDSandwich1/3scanned: Difference between revisions
Appearance
| Line 58: | Line 58: | ||
*'' Ti metal gives asymmetric Ti2p peak shapes'' | *'' Ti metal gives asymmetric Ti2p peak shapes'' | ||
** ''TiO<sub>2</sub> has symmetric peak shapes and TiN has complex peak shape, involving satellite features.'' | ** ''TiO<sub>2</sub> has symmetric peak shapes and TiN has complex peak shape, involving satellite features.'' | ||
* ''Ti2p peak has significantly split spin-orbit components (Δ<sub>metal</sub>=6.1 eV)'' | * ''Ti2p peak has significantly split spin-orbit components (Δ<sub>metal</sub>=6.1 eV)'' | ||