Specific Process Knowledge/Characterization/XPS/Processing/ALDSandwich1/2Survey: Difference between revisions
Appearance
| Line 34: | Line 34: | ||
What to do about this? | What to do about this? | ||
# Continue with the fitting of the high resolution scans - here we will have a much better chancer to work with the fitting of the peaks. | # Continue with the fitting of the high resolution scans - here we will have a much better chancer to work with the fitting of the peaks with intermediate oxidation steps. | ||
# Use a [https://xpssimplified.com/magcis_ion_system.php MAGCIS gas cluster ion source] instead in another instrument to avoid the reducing action of the Ar (single) ion source. | # Use a [https://xpssimplified.com/magcis_ion_system.php MAGCIS gas cluster ion source] instead in another instrument to avoid the reducing action of the Ar (single) ion source. | ||
The analysis continues [[Specific Process Knowledge/Characterization/XPS/Processing/ALDSandwich1/3scanned|'''here''']]. | |||