Jump to content

Specific Process Knowledge/Characterization/XPS/Processing/ALDSandwich1/2Survey: Difference between revisions

From LabAdviser
Jmli (talk | contribs)
Jmli (talk | contribs)
Line 27: Line 27:
[[File:ALD sandwich Ti survey.gif|630px]]
[[File:ALD sandwich Ti survey.gif|630px]]


In the gif file above one can see the etch level in the bottom center right. The fitting routine adds a background to the data and subtracts it from the data before the peak is fitted. This background is shown with a light green color. It is clear that something goes wrong; the fitted backrground eats up the majority of the peak. The result is that the fitted Ti2p peak is much too small - then oxygen is seen as the only peak in the spectrum.
In the gif file above one can see the etch level in the bottom center right.  
 
In the automatic peak fitting routine, a background is added to the data below each peak. This background is then subtracted before the peak is fitted, it is shown with a light green color. It is clear that something goes wrong; the fitted background eats up the majority of the peak. The result is that the fitted Ti2p peak is much too small - then oxygen is seen as the only peak in the spectrum.

Revision as of 14:56, 16 October 2018

Survey spectrum processing

This analysis is continued from here.

Under Display options select 'Stacked Chart View' as seen below. One can see that the peaks in the sandwich emerge and disappear as the depth profile progresses.

Pressing the Automatic Survey ID button will therefore only identify the elements present at each individual level. This is shown below for level 33.

We therefore have to add the remaining peaks manually - this is done by pressing the 'ID' button. In the panel below, select the elements from the periodic table, highlight the peak as shown below with Al2p and press 'Add Peaks'.

Once all the peaks have been added to the peak table, one can create a profile as shown below. Among the profile types choose 'Atomic %'.

In the profile below there is one problem.

As seen above there is only a very small amount of Ti2p. Why is this? Let us zoom in onto the Ti2p peak and see how the fitting goes.

In the gif file above one can see the etch level in the bottom center right.

In the automatic peak fitting routine, a background is added to the data below each peak. This background is then subtracted before the peak is fitted, it is shown with a light green color. It is clear that something goes wrong; the fitted background eats up the majority of the peak. The result is that the fitted Ti2p peak is much too small - then oxygen is seen as the only peak in the spectrum.