Under Display options select 'Stacked Chart View' as seen below. One can see that the peaks in the sandwich.
[[File:ALD-Sandwich-15a.jpg|700px]]

Revision as of 13:47, 16 October 2018

Survey spectrum processing

This analysis is continued from here.