The following links give an approximate oxide time/thickness based on a general formula:
The following links give an approximate oxide time/thickness based on a general formula:


* [https://www.cleanroom.byu.edu/OxideTimeCalc Know thickness - calculate oxidation time]
* [https://cleanroom.byu.edu/oxidetimecalc Know thickness - calculate oxidation time]


* [https://www.cleanroom.byu.edu/OxideThickCalc Know time - calculate oxide thickness]
* [https://cleanroom.byu.edu/oxidethickcalc Know time - calculate oxide thickness]


===Deal-Grove parameters===
===Deal-Grove parameters===