Specific Process Knowledge/Thin film deposition/Deposition of Niobium: Difference between revisions
Appearance
| Line 78: | Line 78: | ||
|-style="background:WhiteSmoke; color:black" | |-style="background:WhiteSmoke; color:black" | ||
! Comment | ! Comment | ||
| | | Substrates will get heated during a longer deposition. During a 100 nm deposition at 2 Å/s, the substrate reached about 105 °C. | ||
| | | | ||
|} | |} | ||