Specific Process Knowledge/Thin film deposition/thermalevaporator: Difference between revisions

Reet (talk | contribs)
Reet (talk | contribs)
Line 39: Line 39:
!style="background:silver; color:black" align="left" valign="top" rowspan="4"|Performance
!style="background:silver; color:black" align="left" valign="top" rowspan="4"|Performance
|style="background:LightGrey; color:black"|Film thickness||style="background:WhiteSmoke; color:black"|
|style="background:LightGrey; color:black"|Film thickness||style="background:WhiteSmoke; color:black"|
*10Å - 1µm* 
*10Å - 1µm
|-
|-
|style="background:LightGrey; color:black"|Deposition rate
|style="background:LightGrey; color:black"|Deposition rate
Line 88: Line 88:
|-  
|-  
|}
|}
'''*''' ''For thicknesses above 600 nm, please request permission.''