Specific Process Knowledge/Thin film deposition/Deposition of Copper: Difference between revisions
Appearance
| Line 79: | Line 79: | ||
|-style="background:WhiteSmoke; color:black" | |-style="background:WhiteSmoke; color:black" | ||
! Comment | ! Comment | ||
|As of August 2018, Cu has not yet been deposited in this machine. | |As of August 2018, Cu has not yet been deposited in this machine. | ||
Please contact the Thin Film group to develop a process. | |||
| | | | ||
|} | |} | ||
Revision as of 13:51, 29 August 2018
Feedback to this page: click here
Deposition of Cu
Copper can be deposited by e-beam evaporation, sputtering or electroplating. In the chart below you can compare the different deposition equipments.
| E-beam evaporation (Temescal) | Sputter deposition (Lesker) | |
|---|---|---|
| General description | E-beam deposition of Cu
(line-of-sight deposition) |
Sputter deposition of Cu
(not line-of-sight deposition) |
| Pre-clean | Ar ion bombardment | RF Ar clean |
| Layer thickness | 10Å to 1µm* | 10Å to 1µm** |
| Deposition rate | 1Å/s to 10Å/s | ~1Å/s |
| Batch size |
|
|
| Allowed materials |
|
|
| Comment | As of August 2018, Cu has not yet been deposited in this machine.
Please contact the Thin Film group to develop a process. |
** To deposit layers thicker than 600 nm permission is required to ensure that there is enough metal (contact metal@danchip.dtu.dk)
* To deposit layers thicker than 200 nm permission is required to ensure that there is enough metal (contact metal@danchip.dtu.dk)
Studies of Cu deposition processes
Roughness of Cu layers - Roughness of Cu layers deposited with Alcatel