== Chromium deposition ==
== Chromium deposition ==
Chromium can be deposited by e-beam evaporation and sputter deposition. It should be noted that in e-beam evaporation, chromium does not melt but evaporates directly from the solid phase. In the chart below you can compare the different deposition equipment.
Chromium can be deposited by e-beam evaporation and sputter deposition. It should be noted that in e-beam evaporation, chromium does not melt but evaporates directly from the solid phase. In the chart below you can compare the different deposition equipment.