s1= s2 = s3 = s, the resistivity is given by: | s1= s2 = s3 = s, the resistivity is given by: | ||
ρ = 2aπs*V/I | |||
where a is the thickness correction factor for thicknesses t equal to or less than half the probe spacing (t=s < 0:5): | where a is the thickness correction factor for thicknesses t equal to or less than half the probe spacing (t=s < 0:5): | ||